SHANGHAI MICROCRE OPTICS-MECH TECH CO., LTDAbout MICROCRE400-812-7833
HVS-30M · 1
HVS-30M · 2
HVS-30M · 3
3D turntable
1 / 3
MODEL · HVS-30M

HVS-30M · Vickers hardness testers

Explore the original technical specifications, related methods and configuration options. Chinese source specifications are retained for accuracy.

Product description

Measuring range: small, thin and surface-coated/plated specimens, as well as brittle yet hard materials such as glass, ceramics, agate and synthetic gemstones. An ideal hardness tester for research and inspection at research institutes, enterprises and quality control departments.

Performance features:

  • Automatic test force loading/unloading mechanism; dwell time freely selectable from 0~60 seconds
  • Computer software programming enables conversion between Vickers and Knoop scales.
  • A stable optical measuring system with adjustable measurement light source intensity.
  • The touchscreen panel displays hardness values directly, offering easy operation and high measurement accuracy.
  • Test results and processed data are stored automatically and can be output via a computer printer.

Specifications

ParameterValue / description
ModelHVS‑30M
Turret typeManual turret
Loading mechanismDead-weight loading
Elevation mechanismPrecision trapezoidal lead screw
Hardness displayTouch screen
HVS-30M test force(30Kg):1kgf、3kgf、5kgf、10kgf、20kgf、30kgf;
Scale conversionHV、HK、HBW、HRA、HRB、HRC、HRD、HRF、HR15N、HR30N、HR45N、HR15T、HR30T、HR45T
Test force applicationFully automatic (loading / dwell / unloading)
Applicable standardsGB/T4340 national standard, ISO6507 quality certification, ASTM standard
Theoretical hardness range8 - 3000HV
Hardness reading methodStandalone measurement by the main unit
Eyepiece magnification10X (digital eyepiece)
Objective magnification(5Kg, 10Kg):10X, 20X (observation, measurement), (30Kg, 50Kg):10X (observation, measurement)
Total magnification(5Kg, 10Kg):100X, 200X (observation, measurement), (30Kg, 50Kg):100X (observation, measurement)
Readout modeEncoder-based reading acquisition
Calculation modeAutomatic calculation
Minimum increment0.06μm (10X objective), 0.03μm (20X objective)
Dwell time0 - 60 s, minimum increment 1 s
Max. specimen height245mm
Indenter centre to inner wall138mm
Supply voltageAC 220V/50Hz
Dimensions570*250*680mm (L*W*H)
Net weight46.0kg
Gross weight61.0kg
(30Kg)1kgf、3kgf、5kgf、10kgf、20kgf、30kgf
(5Kg、10Kg)10X, 20X (observation, measurement), (30Kg, 50Kg):10X (observation, measurement)
Touch screenHVS-30M test force
Specifications, options and final delivery conditions follow the confirmed technical agreement and factory documents; verify any model discrepancy with an engineer.

Related methods & standards

Vickers hardness: from indentation to hardness profiles ↗Brinell hardness: assessing a larger material region ↗Rockwell hardness: interpreting two depth readings ↗Knoop hardness: elongated indents and layer limitations ↗Instrumented indentation: from load–depth curves to contact properties ↗Rockwell hardness and hardened case evaluation: method essentials and limits ↗Brinell hardness on coarse cast structures: method essentials and limits ↗Vickers hardness profile and case depth: method essentials and limits ↗Microhardness matched to coating thickness: method essentials and limits ↗Knoop hardness on brittle ceramics: method essentials and limits ↗Leeb hardness in the field and conversion checks: method essentials and limits ↗Shore and Barcol hardness on elastomers: method essentials and limits ↗Limits of Rockwell to Brinell conversion: method essentials and limits ↗Indentation size effect and load selection: method essentials and limits ↗Hardness mapping across a weld heat-affected zone: method essentials and limits ↗Effective case depth of carburised layers: method essentials and limits ↗Induction-hardened depth and transition zone: method essentials and limits ↗Nitrided layer hardness and brittleness rating: method essentials and limits ↗Laser-hardened track overlap evaluation: method essentials and limits ↗Hardness anisotropy in additively manufactured parts: method essentials and limits ↗Hot hardness and softening onset: method essentials and limits ↗Low-temperature hardness and ductile-brittle transition: method essentials and limits ↗In-situ vacuum high-temperature indentation: method essentials and limits ↗Separating coating hardness from substrate effect: method essentials and limits ↗Daily verification with reference blocks: method essentials and limits ↗Indenter geometry and area-function calibration: method essentials and limits ↗Uncertainty budget for hardness measurement: method essentials and limits ↗Empirical hardness to tensile strength correlation: method essentials and limits ↗Hardness sampling on small and thin parts: method essentials and limits ↗

GB / Chinese standards

GB/T 11354-2005 ↗GB/T 18449.1-2024 ↗GB/T 2654-2008 ↗GB/T 4340.1-2024 ↗GB/T 4340.2-2012 ↗GB/T 5617-2005 ↗GB/T 9450-2005 ↗

ISO

ISO 2639:2002 ↗ISO 4545-1:2017 ↗ISO 6507-1:2023 ↗ISO 6507-2:2018 ↗

Topic-based references do not certify this model or establish full conformity. Confirm the applicable edition, configuration and test conditions.

SCIENCE / HVS-30M

Explore research with this instrument.

Open series research profile ↗

Scientific detail below is the Chinese source edition; reviewed full translations are pending.

Series-level guidance · Measurement and analysis · Confirm model capabilities, accessories and specifications.

Working principle & animation

A square-based pyramid indenter forms a residual indentation under a specified force and dwell time. Measure the two diagonals and use their mean length to evaluate local resistance to indentation.

The schematic explains the basic mechanism; it is not a structural drawing of this model, an operating instruction or a measured result.

Indentation measurement

Schematic model, not device footage or experimental data.

HV = 0.1891 F / d²
SymbolMeaningUnit
FTest forceN
dMean length of the two diagonalsmm
  • With a suitable Vickers indenter, the indentation outline can be read reliably.

Research objects & questions

  • Metal cross-section
  • Surface-hardened layer
  • Weld heat-affected zone
  • Is there a reproducible hardness gradient with depth?
  • Do microstructural changes correspond to indentation positions?

Testing & operation workflow

Follow inputs, actions, outputs and quality gates.

  1. 01

    Define the object and outcome

    Define the research question: Is there a reproducible hardness gradient with depth?; Do microstructural changes correspond to indentation positions? Write the sample identity, target outcome and required configuration into the test plan.

    Input
    Sample information, technical drawings / study protocol and documentation for this model
    Output
    A record specifying the object, outcome definition and available configuration
    Quality check
    Required functions are evidenced in the specific model and accessories; unverified functions remain to be confirmed
  2. 02

    Prepare samples and conditions

    Grind, polish and mark the section orientation, preserving the edge to be measured; avoid mistaking etch pits for indentation boundaries.

    Input
    Defined research object and sample information
    Output
    Traceable samples and preparation conditions
    Quality check
    Edge and microstructure not damaged by preparation
  3. 03

    Check references and equipment

    Check force, indenter and readout chain with a suitable hardness block; calibrate pixel scale for the objective.

    Input
    Prepared samples, reference specimens and equipment records
    Output
    Verification records and availability status
    Quality check
    Reference block range matched to the test force
  4. 04

    Establish the method and procedure

    Select test force and dwell time by material, layer thickness and indentation spacing; save the point plan.

    Input
    Verification results and actual available configuration
    Output
    Saved conditions, parameters and termination rules
    Quality check
    Indentation spacing and specimen thickness comply with the method requirements
  5. 05

    Execute and save raw records

    Apply the load perpendicularly and hold; after unloading measure the two diagonals separately and save the original images.

    Input
    Approved test procedure and quality control settings
    Output
    Raw data, process conditions and anomaly records
    Quality check
    Indentation complete with distinguishable diagonal endpoints
  6. 06

    Review results and model

    Check diagonal difference, boundaries and indentation overlap; report single-point values and positional distribution.

    Input
    Raw signals, reference data and method definition
    Output
    Results with applicability limits and review records
    Quality check
    Do not substitute cross-scale conversions for original results
  7. 07

    Archive and reproduce

    Archive the sample ID, model/accessories, raw records, processing version and anomaly handling with cross-references. Re-measure under identical conditions or check disputed results against the reference method.

    Input
    Reviewed results, raw records and configuration list
    Output
    Traceable research/process records and follow-up verification items
    Quality check
    Teaching calculations, demonstration simulations and real measured data are clearly distinguished; unverified items in the materials are not presented as performance commitments.

Workflows & applications

  • Application object: metal cross-section; research objective: Is there a reproducible hardness gradient with depth?
  • Application object: surface-hardened layer; research objective: Do microstructural changes correspond to indentation positions?
  • Application object: weld heat-affected zone; research objective: Is there a reproducible hardness gradient with depth?

Methods & standards

  • Vickers optical indentation hardness

GB/T 4340.1 Metallic materials — Vickers hardness test — Part 1: Test method

Index of method scope; the version adopted and specific clauses must be verified; this does not constitute certification or a declaration of conformity for this model.

Official source ↗

ISO 6507-1 Metallic materials — Vickers hardness test — Part 1: Test method

Index of method scope; the version adopted and specific clauses must be verified; this does not constitute certification or a declaration of conformity for this model.

Official source ↗

Verify the edition, specimen and configuration. Links do not constitute certification or a conformity claim.

Calculations & simulation

Scientific literature connection

Links indicate related methods or research objects, not evidence that a paper used our instruments.

Resources, service & limits

  • Check force, indenter and readout chain with a suitable hardness block; calibrate pixel scale for the objective.
  • Indentation spacing and specimen thickness comply with the method requirements
  • Verify the delivered model, required accessories, method scope and raw data output; do not infer performance from the series name.
  • In the formula, force is in N and the diagonal in mm.
  • A single-point hardness value cannot be directly converted into strength or fracture toughness for all materials.
  • This dossier covers principles and research workflow; the absence of a measuring-range statement on the page does not mean the device has no limits: the specific range and configuration are subject to technical verification.

Similar instruments

Other models in Vickers hardness testers and the same instrument family.

Browse the whole family ↗

Your next research question. Let’s explore.

Tell us about your material, specimen and measurement goal.

Discuss your application ↗
Find your instrument
⌕
Search products, cases, solutions, standards and literature.