Vickers hardness estimate

HV = 0.1891 × F / d²; d = (d₁ + d₂) / 2

Illustrative example: F=9.807 N and d₁=d₂=0.100 mm give approximately 185.45 HV.

Enter both measured indentation diagonals. This tool calculates a value only; it does not assess indentation validity, thickness, spacing, dwell time or uncertainty. The accepted diagonal range is 0.020–1.400 mm; do not extrapolate to nanoindentation.

Brinell hardness estimate

HBW = 0.102 × 2F / [πD(D − √(D² − d²))]; d=(d₁+d₂)/2

Illustrative example: F=29420 N, D=10 mm and d₁=d₂=4 mm give approximately 228.83 HBW.

This tool accepts the common ball diameters 1, 2.5, 5 and 10 mm and requires a mean indentation diameter of 0.24D–0.60D. A result does not verify the prescribed force/ball combination, specimen thickness or indentation quality.

Engineering stress

σ = F / A₀

Illustrative example: 10000 N / 20 mm² = 500 MPa.

Use the original area before loading. This is engineering stress, without post-necking true-area, local stress-concentration or multiaxial corrections. One load point cannot identify yield strength.

Engineering strain

ε = ΔL / L₀ × 100%

Illustrative example: an extension of 0.5 mm over a 50 mm gauge gives 1% engineering strain.

Obtain ΔL from an extensometer or validated image measurement over the specified gauge. Crosshead displacement includes machine/fixture compliance and slip and is not automatically the gauge extension.

Nominal three-point bending stress

σf = 3FL / (2bh²)

Illustrative example: F=100 N, L=40 mm, b=4 mm and h=3 mm give 166.67 MPa.

For a centrally loaded, simply supported rectangular beam in small deflection. Thickness is measured in the loading direction. Check material-specific span/depth ratio, roller diameter, notches and large-deflection corrections separately; a fracture stress requires the fracture load.

Small angle to height difference

Δh = L × tan[θ × π / (180 × 3600)]

Illustrative example: a 100 mm step and 1 arcsecond inclination correspond to approximately 0.484814 µm height difference.

Enter the actual surface inclination. This is a geometric conversion, not the autocollimator focal-plane spot displacement; reflection doubles the beam deflection. Straightness also requires multiple steps and reference fitting.

Theoretical lateral optical resolution

r = 0.61λ / NA

Illustrative example: λ=550 nm and NA=0.65 give a theoretical resolution distance of approximately 0.516154 µm.

Uses the Rayleigh approximation for an ideal diffraction-limited system. Illumination aperture, aberrations, contrast, pixel sampling and environment also matter. This is not measurement accuracy.

Uniform-temperature linear expansion

ΔL = ᾱ × L₀ × ΔT

Illustrative example: an assumed mean coefficient of 12 µm/(m·K), length 100 mm and uniform rise 10 K give 12 µm expansion. The coefficient is an example input, not a certified material value.

For an unconstrained, uniform-temperature, one-dimensional estimate with a known interval mean coefficient. Heated rods often require integration along temperature gradients. This formula cannot predict complete instrument drift or thermal stress.

Calculations by measurement task

Your next research question. Let’s explore.

Tell us about your material, specimen and measurement goal.

Discuss your application ↗
Find your instrument
⌕
Search products, cases, solutions, standards and literature.