Metallographic preparation checklist: scratches, rounding, artefacts

Check cutting, mounting, polishing and cleaning in order to locate most preparation problems.

2026-10-15

Article

Scratches usually come from skipped grit steps or contaminated consumables; rounding from low mounting pressure or over-polishing; dark spots and false inclusions from incomplete cleaning or over-etching.
Fix programme numbers, log consumable batches and compare at one magnification.
Keep the original cut face and a spare specimen for disputed samples.